CMH35/T/UVC/U/830/G12 35w 3000k ceramic metal halide 2 pin G8.5
Metal halide lamps, traditionally made with quartz arc tubes, are prone to colour shift through life and lamp-tolamp colour variation. Some of the dose, e.g. sodium, (an important component of metal halide lamps), can migrate through quartz to cause colour shift and loss of light through life. The ceramic arc tube resists this material loss, can be manufactured to tighter tolerances and withstands a higher temperature to provide a more constant colour.